Fibra de Vidro e Resina
Tem excelentes propriedades mecânicas, excelente adesão a tubos existentes e sem necessidade de pré-revestimento
- Intervalo de diâmetros publicado
- DN100–1000(4–40″)
- Modelos publicados
- 10 modelos
- Consultar stock e prazo de entrega
- Tamanhos personalizáveis
- Atestado EU TEST
Detalhes
Fiberglass pipe repair uses resin-impregnated reinforcement for a localized patch inside the host pipe. The published pipe patch repair materials include resin components A and B and fiberglass grades EMK600/450, EMK800/300 and EMK800/450. Confirm repair dimensions, formulation, temperature and packer before ordering; materials are configured per repair.
Uma linha de fibra de vidro reforçada impregnada com uma resina especial estabelece uma ligação mecânica ao tubo hospedeiro que elimina a infiltração de água e cria uma reparação estruturalmente reabilitada.
Confirme com a Reliance dimensões, materiais, limites operacionais, documentos de inspeção, disponibilidade e condições de entrega de cada projeto.
Especificações Técnicas
Apenas pré-seleção. A dimensão não confirma a adequação; material, defeito, pressão e acesso exigem avaliação técnica.
Embalagens
| Artigo | Embalagem(kg) | Unidade |
|---|---|---|
| Resina | 40.5 | por conjunto |
| Fibra de vidro | 50 | por rolo |
Dosagem por diâmetro de tubo
- Comum a todos os modelos
- Largura da fibra de vidro
- 125 cm
| Tamanho | Comprimento da fibra de vidro(cm) | Área(m²) | Reparações por rolo | Resina A(mL/kg) | Resina B(mL/kg) | Resina total(kg) | Reparações por conjunto de resina |
|---|---|---|---|---|---|---|---|
| 35 | 0.44 | 108 | 175/0.27 | 350/0.44 | 0.71 | 56 | |
| 55 | 0.69 | 69 | 275/0.42 | 550/0.67 | 1.09 | 36.5 | |
| 70 | 0.88 | 54 | 350/0.55 | 700/0.86 | 1.41 | 28 | |
| 90 | 1.13 | 42 | 450/0.7 | 900/1.1 | 1.8 | 22 | |
| 110 | 1.38 | 34 | 550/0.85 | 1100/1.35 | 2.2 | 18 | |
| 140 | 1.75 | 27 | 700/1.08 | 1400/1.72 | 2.8 | 14 | |
| 175 | 2.19 | 21 | 875/1.36 | 1750/2.14 | 3.5 | 11 | |
| 210 | 2.63 | 18 | 1050/1.63 | 2100/2.57 | 4.2 | 9.5 | |
| 300 | 3.75 | 12 | 1400/2.15 | 2800/3.55 | 5.7 | 7 | |
| 400 | 5.00 | 9.5 | 2000/3.1 | 4000/4.9 | 8 | 5 |
Fibra de vidro e resina necessárias para uma reparação, conforme publicado no folheto.
Resina
| Parâmetro | Componente A | Componente B |
|---|---|---|
| Aparência | Transparente ou amarelo pálido | Castanho |
| Viscosidade a 25°C (mpa.s) | 350-750 | 250-600 |
| Densidade (g/cm3) | 1.52 | 1.2 |
| Ponto de Inflamação (Vaso Fechado) | >200°C | >200°C |
| Estabilidade | Estável à temperatura ambiente | Estável à temperatura ambiente |
| Período de Armazenamento do Produto | 12 meses | 12 meses |
Manuseamento da resina
| Parâmetro | Índice |
|---|---|
| Proporção de Mistura (Volume) | A:B=1:2 |
| Tempo de Mistura e Agitação (min) | 1-2 |
| Tempo de Pega Inicial a 25°C (min) | 10-20 |
| Tempo de Cura a 25°C (min) | 40-60 |
Formulações sazonais
| Parâmetro | Tempo de trabalho(min) | Tempo de cura(min) |
|---|---|---|
| Verão | 20 | 40 |
| Primavera | 25 | 60 |
| Inverno | 30 | 90 |
Tempo de trabalho e de cura por formulação; o folheto não indica a temperatura de ensaio.
Ensaios mecânicos
| Parâmetro | Resultado(MPa) |
|---|---|
| Resistência à flexão | 142 |
| Módulo de flexão | 9215 |
| Resistência à compressão | 164 |
Resultados indicados no folheto. Solicite a documentação dos ensaios para a qualificação do projeto.
Tecido de fibra de vidro
| Parâmetro | Peso Total da Área (g/m2) | Camada de Roving Tecido (g/m2) | Camada de Fios Cortados (g/m2) | Fio de Poliéster (g/m2) |
|---|---|---|---|---|
| EMK600/450 | 1060.71 | 600 | 450 | 10.71 |
| EMK800/300 | 1110.71 | 800 | 300 | 10.71 |
| EMK800/450 | 1260.71 | 800 | 450 | 10.71 |
Especificações da lista de preços atual e dos folhetos de produto da Reliance. Confirme a configuração com a nossa equipa antes de encomendar.
Como funciona dentro do tubo
Ilustração simplificada, fora de escala. Selecione pelo diâmetro interno medido e pela tabela de modelos.
Guia do produto
Guia técnico do folheto em inglês
Fiberglass pipe repair and pipe patch repair materials
Fiberglass impregnated with repair resin forms a localized repair against the host pipe. The brochure describes a mechanical bond to the pipe and applications including clay, cast, PVC and wood pipes.
The online specification tables cover resin components A and B, operating parameters and three fiberglass grades: EMK600/450, EMK800/300 and EMK800/450.
What should a pipe repair kit include?
A pipe repair kit enquiry needs an itemized scope. Specify the fiberglass grade and quantity, resin components and formulation, intended patch dimensions, and whether you also need a repair packer, air hose, pressure gauge and preparation tools. These are separate items to confirm in the quotation, not a published fixed kit.
For Middle East projects, include the destination, planned storage and installation temperatures, quantity and required date. Ask for the applicable resin technical data and handling instructions; a seasonal product name alone does not establish the usable working time at your site.
Preparing the repair material
The brochure describes the following preparation sequence.
Prepare a measuring cup, scraper, mixing bucket and stirrer.
Cut the fiberglass for the pipe diameter being repaired.
Measure components A and B at a 1:2 volume ratio and stir promptly and evenly; the brochure recommends an electric mixing tool.
Pour the mixed resin onto the fiberglass promptly rather than storing it in the bucket. Spread it evenly with a scraper; the brochure states 1.5–2 kg per square metre of fiberglass.
Fold the material to the designed repair thickness, using at least three layers and applying resin at each fold so that it penetrates the fiberglass.
Formulations and material quantities
The brochure lists a 12-month storage period for both resin components. Its packaging table gives component A as 15.5 kg / 10 L and component B as 24.5 kg / 20 L.
The dosage table is the brochure’s planning reference for fiberglass rolls described as 38 metres and 50 kg per roll. Confirm the formulation, repair length, thickness and site temperature for the intended repair.
Matching pipe repair packers
A resin and fiberglass point repair is placed with a pipe repair packer. Packer size, repair length and bypass are selected separately from the resin and fiberglass materials.
Middle East / GCC enquiries
The Dubai office coordinates regional enquiries: TH65 Alandulus, Jumeirah Golf Estate, Dubai, United Arab Emirates. Fiberglass and resin for localized pipe patches are manufactured in China. Reliance is headquartered in Wenzhou, with manufacturers in Qingdao.
Qatar, Saudi Arabia and the United Arab Emirates are listed customer countries. Send enquiries for those destinations, and for other countries, to sales@reliancetrenchless.com or WhatsApp +86 188 6774 8857. Reliance exhibited at Trenchless Middle East 2024, Dubai, UAE.
These materials form a localized resin-impregnated fiberglass patch inside the host pipe. Instant-Lock sleeves and internal joint seals are separate products. The dosage table lists 10 sizes, DN100–1000 (4–40 in). Published grades are EMK600/450, EMK800/300 and EMK800/450, and resin is mixed at A:B = 1:2 by volume. Select the repair packer separately. A seasonal formulation name does not set the working time; include the planned storage and installation temperature.
Export orders are wrapped, labelled and crated on pallets. Air freight is fast air cargo for urgent or time-sensitive orders; sea, land and rail are also published routes. Availability and delivery are confirmed per project.
Measured internal diameter or DN, and the pipe material.
Defect length, and the intended patch length and number of layers.
Fiberglass grade if known, the seasonal resin formulation, and the planned storage and installation temperature.
Whether a repair packer and its accessories are also needed.
Destination country or port, quantity, and the target date.
Whether the order is urgent (air freight) or standard (sea).
Fonte: PDF · 1–2
Estudos de caso
Fotos e vídeos de projetos de pedidos e instalações da Reliance.
Vídeos explicativos
8Vídeos curtos
8Embalagem e entrega
Como os pedidos são embalados e carregados para envio.
Documentos originais
Leia o guia e as especificações online. Os arquivos originais continuam disponíveis abaixo.
A EU TEST verificou os dossiês técnicos de seis dos nossos grupos de produtos face à legislação e às normas UE indicadas. São atestados voluntários, não certificados de organismo notificado.
Guias de compra
Como escolher um packer para reparação de tubagens
Mangas de reparação em aço inoxidável versus remendos de resina e fibra de vidro
Resina para reparação de tubos: vida útil da mistura, presa e cura
Lista de verificação do equipamento para reparação pontual de esgotos
Especificações do reforço de fibra de vidro para reparação pontual
Reparação pontual versus revestimento CIPP de comprimento total
O que é reparação de tubagens sem vala? Métodos e limites
Visão geral das aplicações
Consulte mangas de bloqueio, fibra de vidro e resina e packers para reparação localizada sem abertura de valas.
Sistemas de reparação pontualAplicaçõesConsulta técnica
Inclua estes dados na consulta sobre o produto para que a Reliance possa analisar o pedido.
Diâmetro, material e defeito ou tarefa prevista
Produto ou modelo, dimensões e quantidade
Pressão, condições de serviço, acesso e limitações de instalação
Norma, documentos de inspeção, destino e data pretendida
Confirme com a Reliance dimensões, materiais, limites operacionais, documentos de inspeção, disponibilidade e condições de entrega de cada projeto.
Pedir orçamento: Fibra de Vidro e Resina